presents the results of the chemical, thermal, and corrosion stability tests on AgNW/PET and GO/AgNW/PET after exposure to water for 10 min, acetone for 10 min, isopropyl alcohol for 10 min, or H2S for 20 min. Despite the extreme environment, the electrical conductivity of the GO/AgNW/PET, especially for anti-sulphuration, was excellent and was superior to that of the AgNW/PET