Fig. 7 shows the influences of the applied stress on the surface morphology of the 5 vol. % CNTs/Al composite formed using the SPS process and then exposed to 10 min - hydrolysis in 10 wt. % NaOH solution.
Fig. 7 shows the influencesof the applied stress on the surface morphology ofthe 5 vol. % CNTs/Al composite formed using the SPS processand then exposed to 10 min - hydrolysis in 10 wt. % NaOHsolution.