For testing ohm resistance, To say that the aluminum of IIT use pure aluminum coating, Effect to fire resistance is better. If have ohm resistance can to say IIT use pure aluminum coating. If don’t have ohm resistance can say not pure aluminum coating.
And yesterday was to find a way to fix your product. Guidelines for corrective action.
1. Trial compare between Infrared Heater, Hot air, Heater plate (Direct touch)
Priority test hot air in the first, Hot air can be controlled better infrared and direct touch.
2. Preparation of a new winding machine. Usually is used as an exporter of aluminum two-sided. Emboss 2 side, if first round of emboss, edges are not straight. Effect to second round have wrinkle.
3. Preparation of a new slitting machine due to current machine IIT use, that require employees on the job. Width of machine not able to support job, need to take the guide edge out a waste of time.