This alone shows a promising improvement upon the addition of the sealant layer. However, when the amount of polyols is further increased to 1.6%, the rate of urea release increases by less than 10% from 2.54 to 2.78 mol/L. This comes from an increase in the number of O H functional groups in the polyols and a decrease in the hydrophobicity of the coated samples.