since the interlayer distance of
the powder samples increases with increasing PP content,
it is reasonable to suppose that the x value of the solid,
obtained for an H2PP molar fraction of 0.05 in the
mother solution, is lower than that of the solid obtained
for an H2PP molar fraction of 0.125, that is x < 0.43.