Two new dies were manufactured, D08 and D09 ofTable 2, according to the design A(M) with HIP as fitting method. Unfortunately, the hardness of these stellites after the bonding was over 70HRc.
Two new dies were manufactured, D08 and D09 ofTable2, according to the design A(M) with HIP as fittingmethod. Unfortunately, the hardness of these stellites afterthe bonding was over 70HRc.