let it mixed for 30 – 120 minutes. Let it cool down and ground it
with grinding machine. The ground composites materials were
pressed at 100 MPa and 190o
C for 6 minutes. After samples
were put into mold, appropriate heating, pressure and time were
set and followed by cooling at same pressure and time.[7]