For preparation of ceramic blocks,the mixture of precursor powders
stabilized at 700 1C and polyvinyl alcohol water solution binders
was uniaxially pressed at 200 MPa and then the compact samples
were also sintered at 1000 1C for 1h with thes ame heating rate