Moreover, both types of mixed cement mortars had similar
compressive strengths: 424.5, 385.6 and 361.3 kg/cm2 for coconut
coir fiber, and 376.6, 351.4 and 288.5 kg/cm2 for oil palm fiber,
with fiber replacement ratios of 5%, 10% and 15% by weight, respectively.