contains SEM images of selected specimen fracture surfaces in liquid nitrogen. The melt composite 5% M shows much better NFC distribution in the PBS matrix than 5% S (Fig. 3a and b). Sample, 5% S, shows regions that contain almost pure polymer, while the image also shows an agglomeration for NFC. NFC shows good PBS adsorption on the fibril surface at 5 wt.% loadings.