Different concentrations of the P-chitosan, HP and HP–chitosan were electrospun. For P-chitosan combinations, the highest concentration of chitosan that could be electrospun with polyvinyl alcohol using 1% acetic acid, was 1.5%. For HP combinations the highest concentration of honey that could be electrospun with polyvinyl alcohol was 20% honey (Fig. 1a).