(Fritsch 01.703). The size fraction of 2000 þ 250 mmwas collected
for experiments. Samples were chemically analyzed which their
chemical analysis presented in Table 1.
Steel balls used in Sarcheshmeh concentrator plant were
employed as grinding media, which their chemical compositions
presented in Table 2.