In this experiment, calcinations condition was changed to increase
the ceramic quality after the sintering process. Generally,
both Na and K are believed to be volatilized during the calcination
process as a powder state [16,17]. Kim et al. [18] have reported
that there are significant discrepancies of stoichiometry between
surface and inside of sintered specimens.