pass, beyond which the flexural strength and flexural modulus became
relatively unchanged until the seventh pass where the flexural
properties were reduced to their minimum.
Fig. 3. Notched Izod impact energy of WPC profiles re-extruded from WPC
freshfeed, scrap, and their mixture after the first pass of re-processing.