Prior to modification, Au electrodes (polycrystalline gold rod, 99.99%, 2mm diameter) were polished using alumina slurries with particle diameters 0.3m and 0.05m, respectively, and
subsequently cleaned through ultrasonication in distilled water and ethanol, each for 5min