Shows the influence of die and punch radius on the punch force. When the die and punch radius increases to 10 from 4 mm, the punch force increases to 41,850 N from 31,646 N. If the blank diameter is too large, the force that must be transmitted by the wall will be excessive, and thereby cause it to yield and fail. The formability may be expresses as