The results showed significant improvement of water absorption and compressive strength of geopolymer bricks when concrete residue was added. The maximum compressive strength (8.83 MPa) and the minimum water absorption (0.86%) were found in geopolymer bricks with 40% concrete residue. However, All batches of geopolymer bricks could not meet TIS168-2546 specification.