Whereas, during the recycling process, the BET surface area and saturation magnetization values only slightly decreased after two circles, which further confirmed the stability of the K3PO4/Fe3O4 catalyst.
Whereas,during the recycling process, the BET surface area and saturationmagnetization values only slightly decreased after two circles,which further confirmed the stability of the K3PO4/Fe3O4 catalyst.