Results show that the partial replacement of sand aggregates by either type of glass fibre reinforced polymer recyclates improves the mechanical performance of results polymer mortars.
In the case of trial fomulations modified with the coarser waste mix, the best results are achieved with 8% waste weight content, while for fine waste based polymer mortars, 4% in weight of waste content leads to the higher increases on mechanical strengths.