The experimental setup and the thermocouple arrangement diagram are shown in รูปที่4 .
To avoid damage to the thermocouples, they were separated from the sample with a 1-mm graphite layer during the SHS reaction.
The influence of the graphite layer on the measured temperature will be discussed.
The aspect of the eccentric position of the die relative to the coil was thoroughly discussed in a previous study.