Different from the TEA ramp, in the standard preparation of the INP, the layers are
treated by flash thermal treatment at 500 C for at least 5 min. According to the literature [16], in the case of faster heat treatment, the block-copolymer decomposition and crystallization temperatures are expected to be shifted to higher values.