The heating rates were setat 0.1◦C min−1, 0.2◦C min−1, 0.5◦C min−1and 1.0◦C min−1, respec-tively. The results were plotted in Figs. 5–7, and the detailedparameters were summarized in Tables 1–3. By comparison, wefound that, with the increase of the heating rate, the onset tem-perature, peak temperature and maximum heat flow of all kinds ofcotton increased correspondingly