We have some remarks on ORMA (1.50) validation - > page 9 : task list-4
1) If we will start validation on July, we have to start process to purchase Diapon-K-SF. Can you give me the information to place order. (quotation, quantity, ....)
2) In term of set up process and training for dip technology,
>> Can you give us the SAMPLE tinted lenses after tinting (no curing). To practice tinting operator for compensation color for AR lens.
>> For process set up and process control, can you share the dipping time, tolerance of intensity to us.
Note risk points : we never make 50F with dip tinting. / we have to validate 63 colors (7 main colors/ 9 intensities)
3) For validation lens, would you confirm UV process ? is it UV block?
And we worry about intensity 10F + UV process. Because after UV treatment process, intensity will be 8-10% already and yellowish. How to make good tint color ?
So we need to discuss with you on this point.