Flexural data presented in Table 3 was in agreement with the tensile data in Figure 4, showing increase in flexural modulus and decrease in flexural strength when 30% of the WS is added to PLA
Flexural data presented in Table 3 was in agreement withthe tensile data in Figure 4, showing increase in flexuralmodulus and decrease in flexural strength when 30% of theWS is added to PLA