The DP of cellulose,the major component in original WNP, was 380. After the pretreatment, dissolution and regeneration processes, the cellulose in Film only had a light degradation. The DP of its cellulose was still as high as 277, higher than that of cellophane (DP = 230) prepared by a harsh viscose process