The results indicate that
the PLA sample irradiated at 60 C presents the most enhanced
interlayer adhesion strength as it has the most improved horizontal
10% strain, ultimate stress and failure strain. However, the
PLA sample irradiated at 20 C has poorer interlayer adhesion than
control samples