The design of the casting was modified by reducing the number
of fins to 32 and lengthening then to maintain the required heat
transfer area. The fins were also made to be discontinuous by
placing 0.375 inch gaps at about 1.5 inch intervals to aid in breaking
the laminar boundary layer.