In order to obtain optimum analytical parameters, we used SWV to monitor the current signal change (i) (i = i0− i, where i0andi are the reduction peak current intensity of MB tags at −0.22 V in the absence and presence of Hg2+, respectively), which increased with increasing mercury concentration.