Superfine DSF powder (DSF-JM; D50 = 4.3 ± 0.1 lm) was prepared from DSF powder
(DSF-150; D50 = 257.0 ± 1.7 lm) via conventional sifting followed by jet-milling. The jet-milled DSF
showed significant increases in hydration properties, with increases in the water-holding capacity,
water-solubility index, and swelling capacity of 24%, 39%, and 32%, respectively
Superfine DSF powder (DSF-JM; D50 = 4.3 ± 0.1 lm) was prepared from DSF powder(DSF-150; D50 = 257.0 ± 1.7 lm) via conventional sifting followed by jet-milling. The jet-milled DSFshowed significant increases in hydration properties, with increases in the water-holding capacity,water-solubility index, and swelling capacity of 24%, 39%, and 32%, respectively