In general, HTGN has usually been
applied to Cr based austenitic, martensitic and duplex stainless
steels, which have high nitrogen solubility in the austenite phase.
However, the lownitrogen solubility of a ferrite single phase prevents
HTGN of ferritic stainless steel.