the strengths of the composites produced with and without the dispersant were approximately 1.4–1.7 and 0.85 MPa, respectively. Thus, the dispersant still affected the strength of the heated samples.
the strengths of the composites produced with and without the dispersant were approximately 1.4–1.7 and 0.85 MPa, respectively. Thus, the dispersant still affected the strength of the heated samples.