The effectivity of the anticaking agents ferrocyanide, ferricyanide and iron(III) meso-tartrate on the caking of
sodiumchloride was studied at the powder scale and on a two-crystal scale. Using the integrated stirring energy
as ameasure of caking strength of the powders gives results that agreewellwith industrial experiencewith these
anticaking agents. For two single crystals, the required separation force was used as a measure for the caking
strength. In this case, higher dosages of anticaking agents are required to prevent caking. This is caused by an
increase in the number of contact points between the crystals, as was concluded from the surface morphology
of the sodium chloride crystals, which we studied using atomic force microscopy. This change of the surface
morphology is in turn caused by the applied anticaking agents. This shows that it is not only the surface area,
but also the number of contact points, and thus the particle size distribution, which are critical in determining
the optimal dosage of anticaking agents on caking powders.
©