The effect of reactive compatibilization i.e.,
adding 8 phr MA and 2 phr LU to the [PLAþ30% WS] composite
during processing was investigated and compared to the conventional
method of adding 3 or 5 phr of PLA-g-MA as compatibilizer to
the PLA/WS composite during fabrication