Under optimum conditions, the pre-hydrolysis/Kraft pulping with
20% active alkali, 25% sulfidity, and HEHP bleaching resulted in
dissolving pulp with -cellulose content 94.8%, degree of polymerization
279, and ash content 0.75%. The xylose content in jute
stick was lower as compared to hardwood