differences (p 0.05) were appreciated among HAD and 2 W/g and
the rest of the treatments. No differences between 4 and 6 W/g
were appreciated mainly because a low level of mass was reached
caused by water loss; the low level of moisture reached decreases
the effect of MW power. After 60 min of drying, treatments
converged to the threshold of the thermodynamic properties of dry