and the elongation at break increases
sustainedly with the further TBT loading level, and gives the values
of 298% in the case of 0.5% TBT loading. Similar ultimate strain was
also obtained for PLA/PCL blends using isocyannates-lysine
triisocyanate (LTI)[7]and dicumyl peroxide (DCP)[16]as reactive
processing agents