if the slope length is too
long, the slurry could form a solid shell on the slope. On the
other hand, if it is too short, nucleation sites may be
insufficient. Thus, optimum pouring length, promotes the
transformation of coarse dendrites into rosette shape grains
by increasing the cool-shear time