Significant
difference (p < 0.05) was observed in thickness between both CHOLE
and CH-OPE at 20 g L1 and pure CH film due to OOR
phytochemicals. Otherwise, no significant difference (P > 0.05) was
observed between CH films and CH incorporated films with OLE
and OPE at 10 g L