The optimal milling conditions were selected as follows: solid/liquid ratio of 1:10, ball speed of 350 r/min, raw material particle size with 0.5 mm, adding the amount of grinding media and number of balls of 20 (steel ball, Φ=10 mm), 30 min after grinding.