Before fabrication of the composite plaques, PLA pellets (used to mold PLA sheets detailed below) and the flax reinforcements (UD flax or UD flax-paper layers) were oven-dried at 80 C for 12 h. The composite plaques were fabricated in two stages (Fig. 5).