In order to remove MgO and Fe, the obtained products were leached in 1 M HCl solution at room temperature for 30 min. The leached product of this sample is given in Fig. 7(b). It can be seen from this figure that MgO and Fe were completely removed from the powder, but ZrO2 could not be removed.