During this
experimental investigation, neither exfoliation nor graphene formation
were observed. Furthermore, the glassy carbon electrode (GCE) surface
was modified using chemically modified graphite by drop casting
method (1 mg/mL). The modified electrode has been air dried for an
hour and subsequently at 60 °C for 10 min.