Thus, precipitated ZnO nanoparticles were cleaned many times with de-ionized water to remove the byproducts which were bound with the nanoparticles and then dried in air atmosphere at about 70 C for 1 h and annealed at 350 C. Similarly, for sodium doping high purity sodium acetate dehydrate was used for chemical reaction.