When the temperature reached about190∘C,combustion flame appeared.Figure 2 shows the observation of flame during the combustion of nitrate and fuel.After completion of combustion,the crude brown color powder was obtained . The obtained combustion product was annealed at 800∘C for 3hrs in a groove rolled muffle furnace.