the magnitude of both peaks most probably because of the higher
crystallinity of the hydrolyzed cellulosic residue compared to the
original fibers present in cassava bagasse. The degree of crystallinity
was determined and found to be 43.7% and 54.1% for the cassava
bagasse and hydrolyzed residue obtained using conditions CW40,
respectively