By the carbonization process applications at temperatures of 400 degrees as follows: 1. The carbonization process applications at temperatures of 400 degrees stimulation with NaOH at a ratio of 1: 1 for 1 hour, activated carbon has a surface area. a BET pore size and pore volume as high as possible.