After washing, dry biomass was prepared by drying at 55 8C during 24 h and subsequently powdered. The concentration of added biomass was 2 g/l into 100 ml of metal solution for kinetic experiments. Samples were taken from solution after 10 min, 1 h, 6 h and 24 h of processing, filtering and analysis