The kappa number was 21.0 at 14% alkali charge, which was
decreased to 15.2 with increasing alkali charge to 18%. Required
amount of alkali was less to get bleachable grade pulp in prehydrolysed
jute stick. This can be explained by expose of lignin
during pre-hydrolysis process.