preparation of catalyst by dry impregnation support after burn at temperature 550 2 hr to get rid of the impurities than mixed in a solution of sodium carbonate 45% than dry at temperature 120 16 hr the burn temperature 550 5 hr the catalyst received to keep it in oven the moisture before the test reaction