Thus, PS films that were too thick (films
thicker than 0.2% PS with plasma treatment shorter than 60 s, or PS
films fabricated with higher PS concentrations than 0.4% plasma
treated for 0–150 s), were not capable of improving the protein
binding signals in immunoassay, and only ultrathin PS films could
significantly improve the protein bioassay performance.